Formation of dissimilar joints between γ-TiAl titanium aluminide and EP303 steel under friction welding conditions
Zikhor Igor 0000-0001-7780-0688, Koltsov V.V.
0009-0008-6078-1706, Levchuk А. М.
0000-0002-0361-7394, Shylo Yu.A.
0000-0002-6174-5925, Zavertannyi M.S.
0000-0002-8415-8555, Hushchyn K.V.
0000-0003-3298-4537
- E.O. Paton Electric Welding Institute
Oral Online
In the manufacture of turbocharger rotor shafts and bimetallic automotive engine valves, it is essential to obtain welded joints between heat-resistant alloys and structural steels. Titanium aluminide-based alloys are promising materials for use in the automotive engine industry. This determines the relevance of the problem of their welding with ferritic-pearlitic, austenitic, and martensitic steels. The factors limiting the widespread use of titanium aluminides are their high sensitivity to thermal and deformation welding cycles, as well as the risk of cracking, porosity, and the formation of brittle layers with variable chemical composition. The possibility of forming dissimilar joints between gamma-titanium aluminide (Ti-46Al-2Cr-2Nb) and 55X20H9AN4 (EP303) heat-resistant steel under friction welding (FW) conditions was investigated. It was experimentally established that during conventional FW, the temperature in the contact interaction zone exceeds the eutectic point of the Ti-Fe system. Cracks and porosity are observed in the joints. The width of the concentration transition zone in the joint area is about 40 microns; furthermore, regions up to 20 microns wide with a stable chemical composition and high microhardness (5500 HV 0.1) are detected. Porosity is observed in the transition zone on the EP303 steel side, which is caused by the reactive diffusion of alloying elements of the welded materials. It is shown that during hybrid FW, due to the programmed reduction of the peripheral rotation speed and an increase in the forging pressure, a decrease in the contact zone temperature is ensured, resulting in the formation of solid-state dissimilar joints free of pores and cracks. The width of the concentration transition zone does not exceed 8 microns, and no regions with a stable chemical composition were detected.