INCREASING THE SERVICE LIFE OF WELDED JOINTS OF ABSORBING RODS OF THE CONTROL AND PROTECTION SYSTEM OF WWER-1000 REACTORS
Oleh Makhnenko 0000-0002-8583-0163, Oleksiy Milenin
0000-0002-9465-7710, Olena Velikoivanenko
0009-0007-3704-2000, Galina Rozynka
0009-0009-1750-7266, Oleksiy Makhnenko
0000-0003-2319-2976
- E.O. Paton EWI NAS of Ukraine
Oral Online
Absorbing rods (AR) of the control and protection system (CPS) of WWER-1000 nuclear reactors perform protective and control functions depending on their location in the reactor core and are designed to quickly stop the nuclear reaction, maintain power at a given level, transition from one level to another, etc.
The use of absorbers based on dysprosium titanate or dysprosium hafnate in tablet form allows in the future to increase the service life of the AR CPS WWER-1000 to 20-30 years [1]. Therefore, the specified service life of 10 years for the AR design should be extended to ensure the integrity of welded joints and the tightness of the AR shell.
Based on the results of the study of the stress-strain state and the resistance to brittle fracture of welded joint of the shell with a cone [2] for the initial AR design (shell diameter 8.2 mm, wall thickness 0.55 mm, nickel alloy 42KhNM) with an internal hole length of 20 mm in the cone and additional design options with an internal hole length of 10 mm and without a hole, the following recommendations to increase the resistance to brittle fracture have been developed.
Eliminating the internal hole under the welded joint allows, firstly, to significantly reduce the level of maximum residual stresses. Secondly, the influence of internal pressure due to the swelling of the absorber in the reactor shutdown and maximum emergency load modes on the stress state of the welded joint is also reduced.
According to the results of the calculated prediction of the minimum brittle strength safety factor nmin in the cross section of the welded joint of the cone with the shell at different sizes of the postulated crack (material after irradiation, crack size ratio 2a/2c=0.3), reducing the length of the internal hole in the cone to 10 mm allows to significantly increase the resistance to brittle fracture to nmin=2.5; the variant without the internal hole – to nmin=2.9 (the initial design nmin=2.14).
The welding technological parameters also affects the resistance to brittle fracture, namely, welding with preheating up to 150°C allows to increase the minimum safety factor of brittle strength to nmin=2.25; the welding option with increased heat input (150%) is more significant - up to nmin=3.0, due to a decrease in the level of maximum residual stresses. But the additional technological operation of preheating complicates the welding technology, and welding at increased heat input can lead to undesirable residual deformations and the possible formation of hot cracks in the material of a nickel alloy during the welding.
Changing the design of the welded joint by reducing the length or eliminating the internal hole in the cone is a fairly simple and reliable way to increase the resistance to brittle fracture of the welded joint of the shell with the cone and, accordingly, increase the service life of the welded structure of the AR CPS WWER-1000.
References:
1. Grytsyna V.M. Creation of neutron-absorbing materials for control and protection systems of nuclear reactors with increased service life characteristics using domestic raw materials and technologies. Visn. Nac. Akad. Nauk Ukr. 2026. (3), pp.42-51.
2. Milenin O.S., Velikoivanenko O.A., Rozynka G.P., Makhnenko O.O. Features of the stress state of welded absorbing rods of the VVER-1000 control and protection system during production and further operation. Tech. diagnostics and non-destructive testing, 2025, No.3, pp.15-23. (in Ukrainian)