Wetting and brazing of zirconia with TiBraze800 filler
Durov Oleksii1 0009-0007-8264-0333, Stetsyuk Tatyana1
0009-0001-2578-234X, Poliarus Olena2
0000-0003-3181-419X, Shapiro Alexander
0000-0002-3560-7801
- 1Frantsevich Institute for Problems of Materials Science National Academy of Science of Ukraine, Kyiv, Ukraine
- 2Institute of Metallurgy and Materials Science of Polish Academy of Sciences, Krakоw, Poland
Oral Online
TiBraze800 brazing filler (Zr-14.7Ti-12.6Ni-7Cu-1.2Hf wt%) developed for brazing of titanium, demonstrate high adhesion to solid oxides, since it contains adhesive-active elements (titanium, zirconium, hafnium).
Wetting of zirconia with TiBraze800 in vacuum was studied. A contact angle of 35° was achieved at 900 °C for holding time of 3 min, but after 30 min holding, drop deformation and loss of gloss were observed due to melt solidification.
Microstructural studies have shown the formation of transition layers containing highly oxidized titanium and zirconium, i.e. the active components of the melt interact with the oxygen of the substrate according to the scheme zirconium and titanium of the melt interact with the oxygen of the substrate and are oxidized to oxides, with an oxygen-deficient non-stoichiometric phase forming in the substrate. As a result, the alloy composition shifts from the region of existence of the liquid to the solid-phase region. Since sufficient wetting was achieved, TiBraze800 was tested for brazing of zirconia ceramics to itself, as well as to molybdenum and titanium. The shear strength was 79-91 MPa for zirconia/zirconia joints, 71-88 MPa for zirconia/molybdenum joints and 95-118 MPa for zirconia/titanium joints.