FDM 3D Printing of Bioactive PLA+ Structures with a Hydroxyapatite Coating: Mechanical and Thermomechanical Characterization
Ivan Korolkov1 0009-0002-6171-0391, Maksym Iurzhenko1
0000-0002-5535-731X, Valeriy Demchenko1
0000-0001-9146-8984, Oleksandr Lysenko1
0009-0009-8128-0393, Liakhovets Oleksandr1
0009-0009-3858-4578, Sergii Voinarovych1
0000-0002-4329-9255, Sergii Kaliuzhnyi1
0000-0002-8132-3930, Mykhailo Rublenko2
0000-0001-9690-9531, Volodymyr Kolomiiets3
0000-0003-2322-7091, Sergiy Firstov3
0000-0001-9676-722X, Vasyl Shmahoi4
0000-0003-2635-4125, Oleksandr Buryanov5
0000-0002-2174-1882, Oleksandr Slieptsov6
0000-0002-0608-1855, Nadiya Sova7
0000-0003-3550-6135, Bogdan Savchenko8
0000-0002-8636-5734
- 1E.O. Paton Electric Welding Institute, the National Academy of Sciences of Ukraine,
- 2Bila Tserkva National Agrarian University
- 3Frantsevich Institute for Problems of Materials Science, National Academy of Sciences of Ukraine
- 4Medical Center «Dobrobut-Polyclinic»
- 5Bogomolets National Medical University
- 6Kyiv National University of Technologies and Design
- 7Kyiv National University technologies and Design
- 8Kyiv national university technology and design
Oral Online
The study involved a series of computational and experimental procedures aimed at developing bioactive polymer structures with potential for medical applications. The initial stage focused on investigating the properties of polylactide (PLA) and a modified composite variant PLA+. PLA was identified as a promising biodegradable polymer for implant fabrication due to its biocompatibility, lack of cytotoxicity, and suitability for FDM 3D printing.
To conduct mechanical and thermomechanical testing, geometric models were developed using FreeCAD software; these included "dog-bone" tensile specimens as well as solid and perforated tubular structures designed to simulate bone tissue fragments. The specimens were fabricated via FDM 3D printing using a GEMMA 3DP printer, with a layer height of 0.2 mm, a printing speed of 40 mm/s, and a printing temperature of 200°C.
Static uniaxial tensile tests demonstrated that modifying the PLA did not compromise the interlayer strength of the 3D-printed structures. The PLA+ specimens exhibited more consistent mechanical properties and lower result variability compared to the base PLA. For both material types, the ultimate tensile strength was approximately 40 MPa. Dynamic thermomechanical studies conducted in the 20–40°C temperature range under a load of approximately 0.4 MPa demonstrated that perforated structures exhibit more stable behavior during cyclic heating and cooling compared to solid samples. It was found that the level of thermal expansion for PLA+ was approximately 10%, whereas for PLA it was about 6%.
Based on an adapted Burgers viscoelastic model, the relaxation temperatures of the tested samples were calculated. The perforated PLA+ sample demonstrated the best results, with a relaxation temperature of 37.2°C; this corresponds to the temperature range of the human body, indicating the material's potential for use in implant manufacturing.