Heat treatment of laser welded superelastic nitinol wires
Sergii Kedrovskyi1 0009-0000-6381-1511, Yuri Koval1
0009-0005-1977-6807, Victoriia Slipchenko1
0009-0004-3480-5795, Kateryna Soroka1
0009-0008-4863-4172, Olexandra Zatsarna1
0000-0003-3200-7672, Artemii Bernatskyi2
0000-0002-8050-5580, Aleksandr Siora2
0000-0003-1927-790X
- 1G. V. Kurdyumov Institute for Metal Physics of the National Academy of Sciences of Ukraine
- 2E.O. Paton Electric Welding Institute
Oral Online
This study investigates the effect of post-weld heat treatment on the mechanical properties of titanium nickelide (Nitinol) welded joints. The objects of study were superelastic Nitinol wire specimens with a diameter of 3 mm, joined by methods of laser welding in a protective argon atmosphere. To relieve residual stresses and optimize the phase composition of the heat-affected zone (HAZ) and the welded joint, annealing was performed at 450 °C for 1 hour. Mechanical properties were evaluated using tensile and three-point bending test methods.
The experiments have shown that heat treatment has a significant effect on the ductility and fracture behavior of welded joints. When tested using the three-point bending method (60 mm base), the original wire showed complete shape recovery with a deflection of up to 17 mm. Testing of the as-welded (untreated) joints revealed highly unstable mechanical behavior. The specimens underwent brittle fracture at an average deflection of only 7,6 mm. On the deformation diagrams, failure occurred at the very onset of the martensitic plateau (the superelastic region), precisely upon reaching the critical stress for the start of the austenite-to-martensite phase transformation. In all untreated cases, the crack ran strictly through the center of the weld joint, highlighting severe concentrations of residual welding stresses and the presence of brittle dendritic phases within the fusion zone.
Post-weld heat treatment at 450 °C for 1 hour led to a radical improvement in mechanical performance. The maximum deflection before destruction more than doubled, reaching 15,8 mm. The annealed specimens displayed a well-defined, extended phase transformation stage, failing only at the very end of the superelastic plateau (during the transition to elastic loading of the induced martensite phase). Crucially, the crack trajectory shifted: the fracture line no longer followed the weld joint but relocated into the heat-affected zone. This indicates that the annealing successfully relaxed internal stresses within the cast weld structure and enhanced its strength, making the boundary HAZ the new weakest link of the joint system.
Keywords: Nitinol, laser welding, heat treatment, superelasticity, three-point bending, heat-affected zone (HAZ).