← Advanced Technologies of Special Electrometallurgy

Effect of Electroslag Heating on Vanadium Recovery during Aluminothermic Production of FeV80 Ferrovanadium

М.О. Vdovin 0009-0007-4848-4154, Yu.V. Kostetskyi, 0000-0003-0742-0684

  1. E.O. Paton Electric Welding Institute (PWI)Kiev, Ukraine

Poster

Effect of Electroslag Heating on Vanadium Recovery during Aluminothermic Production of FeV80 Ferrovanadium

Abstract. A study was conducted to improve the technological efficiency of FeV80 ferrovanadium production from technical-grade vanadium pentoxide V₂O₅ containing 82–86% of the main component by aluminothermic reduction with secondary aluminum powder followed by electroslag heating of the reduction products. To implement the process, the OV-1901 pilot-scale electroslag remelting unit was modified by introducing a bifilar DC electroslag heating configuration and integrating a thyristor current modulator providing pulsed polarity reversal of the graphite electrodes at a frequency of 2 Hz.

The effect of electroslag holding time on the degree of vanadium recovery was investigated experimentally. After aluminothermic reduction, the degree of vanadium recovery into the metallic phase was found to be 74%. One of the main reasons for incomplete recovery is the hindered separation of the metallic and slag phases due to the entrapment of fine metal prills in the viscous high-alumina slag. Subsequent pulsed bifilar electroslag heating promotes more intensive slag–metal interfacial interaction, coalescence of metal prills, and their sedimentation. After holding for 5 and 10 min, the degree of vanadium recovery increased to 86 and 92%, respectively. The maximum value of 94% was achieved after 15 min of electroslag holding.

At the same time, further extension of the electroslag heating period was found to be limited by intensive thermal and chemical erosion of the P-91 magnesite-brick lining caused by the aggressive high-alumina slag. Considering the degree of vanadium recovery, the efficiency of metal–slag phase separation, and the stability of the refractory lining, a rational electroslag holding time of 10–12 min was established. The proposed processing regime provides increased vanadium recovery and enables the production of FeV80 ferrovanadium with a controlled residual aluminum content.

Keywords: FeV80 ferrovanadium, vanadium pentoxide, aluminothermic reduction, electroslag heating, bifilar configuration, pulsed polarity reversal, vanadium recovery, coalescence, sedimentation.