← Advanced Technologies of Special Electrometallurgy

Electroslag Remelting in Vacuum: Effect of Pressure on Process Stability and Ingot Quality

Igor Protokovilov 0000-0002-5926-4049, Vitalii Porokhonko 0000-0002-6490-7221, Denis Petrov 0000-0003-2937-9299

  1. E.O. Paton Electric Welding Institute

Oral Online

Experimental results of electroslag remelting (ESR) of metallic electrodes in a chamber-type furnace at different pressures in the melting zone, ranging from vacuum to overpressure, are presented.

Experiments were conducted during the production of 65, 85, and 105 mm diameter ingots from steel and VT1-0 (CP titanium Grade 2) and VT22 (Ti-5Al-5V-5Mo-1Cr-1Fe) titanium alloys. Salt fluxes AN-T1 and AN-T4, as well as fluoride-oxide fluxes ANF-1, ANF-6, and ANF-28, were used. The pressure in the working chamber was varied from 3 to 300 kPa. The electrical parameters of the process, gas composition of the ingots, and their macrostructure were analyzed.

The effect of reduced pressure on the stability of the electroslag process was investigated, and the limiting conditions for stable operation were established for different types of fluxes. It was shown that decreasing pressure leads to a reduction in melting current and an increase in the amplitude of its fluctuations. At a critical pressure, boiling of the slag pool occurs, resulting in loss of process stability. The critical pressure was found to depend on the flux composition and remelting power. For AN-T1 and AN-T4 salt fluxes, the critical pressure was 12–22 and 15–26 kPa, respectively, whereas for the fluoride-oxide fluxes ANF-1, ANF-6, and ANF-28, lower values of 3–15 kPa were observed. Increasing the remelting power resulted in a higher critical pressure.

Based on these relationships, ESR of VT1-0 and VT22 titanium alloys using AN-T4 flux was investigated over a pressure range of 20–300 kPa. Stable operation was achieved throughout the investigated pressure range, producing dense ingots free from pores, slag inclusions, and other internal defects. The effect of pressure in the melting chamber on the gas composition of titanium ingots was established. ESR at reduced pressures of 20–25 kPa resulted in a 20–35% reduction in hydrogen content compared with remelting at elevated pressure, whereas no systematic effect of pressure on oxygen and nitrogen contents was observed over the investigated pressure range.

The effect of pressure on the structure of ESR ingots was also established. The VT1-0 ingot produced at 25 kPa exhibited an average equivalent grain diameter of 2.07 mm, compared with 1.26 mm at 160 kPa.

The results demonstrate the feasibility of controlling ESR conditions by varying the pressure in the melting chamber of a chamber-type ESR furnace. This provides a basis for using reduced pressure as a technological parameter, particularly for reducing hydrogen content in titanium ingots.