MICROSTRUCTURAL FEATURES AND MECHANICAL PROPERTIES OF AISI 316L LAYERS FORMED BY LASER DIRECT METAL DEPOSITION

Kushnarova Olga 0000-0002-2125-1795, Berdnikova Olena 0000-0001-9754-9478, Sokolovskyi Mykola 0000-0003-3243-5060, Siora Oleksandr 0009-0005-8542-1633, Bernatskyi Artemii 0000-0002-8050-5580, Frolov Mykhailo 0009-0002-7869-9360, Alekseienko Тetiana 0000-0001-8492-753X, Titkov Yevhenii 0000-0003-2735-6923

  1. E.O. Paton Electric Welding Institute of the NAS of Ukraine

Oral Online

Laser Direct Metal Deposition (L-DMD) is a promising additive manufacturing technology for the localized restoration of critical thin-walled components. It provides a limited thermal effect on the base metal and the formation of a reliable joint. At the same time, the high heating and solidification rates during L-DMD determine the specific features of structure formation and mechanical properties of the deposited layers.

This study investigates the microstructure, local chemical composition, and microhardness of layers deposited via laser deposition during the restoration of 12Х18Н10Т stainless steel samples using AISI 316L powder and a 0.25 mm thick 12Х21Н5Т steel strip. Structural and chemical characteristics of the deposited layers were examined using optical, scanning, and transmission electron microscopy, as well as energy-dispersive X-ray spectroscopy.

The formation of a multilayer system was established, consisting of a 12Х21Н5Т surface layer, an AISI 316L layer, a transition zone, and the 12Х18Н10Т base metal. The deposited layers are characterized by an austenitic-ferritic dendritic structure. The microhardness ranged from 2740 to 3660 MPa for 12Х21Н5Т , 2280 to 3510 MPa for AISI 316L, and 1810 to 3220 MPa for 12Х18Н10Т . The distribution of Fe, Cr, and Ni shows a stable composition within the deposited layer and a smooth transition of element concentrations in the transition zone.

Transmission electron microscopy revealed the formation of a fine cellular austenitic substructure with a cell size of 0.2–0.6 µm, indicating substructural strengthening of the deposited layers. The dislocation density was 2–4×10¹⁰ cm⁻² in the AISI 316L layer and 4–7×10¹⁰ cm⁻² in the 12Х21Н5Т layer. This structure provides both substructural and dislocation strengthening.

Hydraulic testing confirmed the performance of the restored samples, which withstood 24 loading cycles at 48 MPa and a subsequent pressure increase up to 98 MPa without failure.

Thus, L-DMD ensures the formation of a high-quality metallurgical bond, an austenitic-ferritic dendritic structure, and a fine cellular dislocation substructure. The increase in microhardness of the deposited layers is associated with structural and substructural strengthening. The obtained results confirm the viability of L-DMD for restoring critical thin-walled structures.