Thermal Coatings Containing Multiple MAX Phases
N.V. Vihilianska 0000-0001-8576-2095, O.M. Burlachenko
0000-0003-2277-4202, A.P. Murashov
0000-0002-0357-9068, A.O. Yushchenko
0009-0005-6636-8275, O.P. Gryshchenko
0000-0003-2640-8656
- E.O. Paton Electric Welding Institute of the NAS of Ukraine
Oral Online
The Ti3SiC2, Ti3AlC2, Ti2AlC, and Cr2AlC compounds belong to the class of thermodynamically stable MAX phases. The nanolayered structure of these materials provides a combination of properties characteristic of both metals and ceramics. A promising direction for their application is the deposition of coatings using thermal spray (TS) methods. The production of coatings containing two or more MAX phases may improve their properties and expand their application areas. A modern technology for producing powders for TS is mechanochemical synthesis (MChS), using both simple elements and compounds as starting materials.
This work is devoted to studying the formation processes of coatings produced by atmospheric plasma spraying (APS) and high-velocity oxy-fuel spraying (HVOF), containing MAX phases: Ti3AlC2 + Ti3SiC2 and Ti2AlC + Cr2AlC, as well as investigating the properties of these coatings. Composite powders produced by MChS of powder mixtures 75TiAl + 25SiC and 68.5(Ti,Cr)C + 31.5Al (wt.%) were used as starting materials for spraying.
The produced coatings exhibit a fine-grained structure with porosity of 12–14% for APS and ≤2% for HVOF. The phase composition of the coatings does not differ significantly from that of the sprayed materials, and the coatings consist of a metallic matrix (TiAl or Cr5Al8), ceramic inclusions (TiC, Ti5Si3, Ti0.8Cr0.2C), and MAX phases (Ti3AlC2 + Ti3SiC2 or Ti2AlC + Cr2AlC). As a result of the interaction of the sprayed material with oxygen from the surrounding environment, a small amount of titanium oxides (TiO, TiO2) forms in the coatings, which are distributed throughout the coating structure in the form of thin interlayers. The average microhardness of coatings in the TiAl–SiC system is 4310±890 and 5140±1160 MPa, and in the (Ti,Cr)C–Al system is 5370±1480 MPa and 3340±510 MPa for APS and HVOF, respectively.
The heat resistance of the produced coatings, after their exposure in a furnace at a temperature of 800 °C in an air atmosphere for 5 hours, is three times higher than that of AISI 1045 steel under the same conditions and twice as high as that of iron aluminide FeAlCr thermal coatings. The wear resistance of the coatings under dry sliding friction conditions against a counterbody of hardened steel AISI 52100 (hardness ~60 HRC), at a load of 1.86 MPa and sliding velocity of 1.32 m/s over 10 minutes, was found to be comparable to that of NiCrBSi–TiB₂ plasma coating, with a wear rate of 10.73–16.42 μm/km.
The produced coatings can be used as a substitute for NiCrBSi system coatings in friction conditions, as well as for protecting components operating at elevated temperatures.