← Technologies, Filler Materials and Equipment

IMPROVEMENT OF THE PERFORMANCE CHARACTERISTICS OF BUTT JOINTS OF STEELS AND ALLOYS THROUGH THE APPLICATION OF LASER-ARC AND LASER-PLASMA WELDING

Vladyslav 0000-0003-3072-6761, Gui Rong 0009-0009-4733-7974, Yanchao Hu 0009-0009-4834-7680, Oleksandr Bozhok, Angela Oliniychuk, Maxim Pervushin

  1. E.O. Paton Welding Institute of the NAS of Ukraine

Oral Online

When manufacturing structures from modern high-strength aluminum alloys and steels, plasma, TIG, and MIG welding processes are widely used. These processes make it possible to achieve sufficient levels of weld strength and ductility and provide the required service characteristics of the joints. However, their main disadvantage is relatively high residual deformation. To minimize these deformations, it is advisable to maximize the welding speed while maintaining stable weld formation. This can be achieved by establishing a stable synergistic effect through the addition of focused laser radiation to the energy input of the arc heat source. The relevance of applying such a hybrid laser-arc or laser-plasma process lies in the possibility of increasing welding productivity while simultaneously reducing residual deformations and improving the mechanical properties of the joints.

The aim of this work is to develop promising approaches to improving the performance characteristics of butt joints of steels and alloys compared with those produced by conventional arc and plasma welding processes, based on the application of laser-arc and laser-plasma welding processes to reduce the process heat input per unit length and refine the grain structure of the welds.

To achieve the stated objective, a laboratory experimental setup for laser-MIG and laser-PAW welding using fiber laser radiation was developed. Technological studies of laser-MIG and laser-PAW butt welding of AISI 304 steel and 1561 alloy specimens (4 mm thick) were conducted. Based on these studies, the optimum welding parameters were determined according to the criterion of achieving the maximum welding speed while maintaining high-quality weld formation (Class C or B according to ISO 10042). Residual deformations of the welded specimens were measured by moving them over a flat steel plate relative to the probe of a dial indicator, which was stationary mounted on a stand.

It was determined that, owing to the synergistic effect achieved during hybrid welding, an increase in the process heat input per unit length by approximately 60% can result in a 2–3-fold increase in welding speed. The effect of the welding parameters on the magnitude of residual deformations, microstructural features, and the strength of the joints under static tensile testing was determined.