Laser forming and strengthening treatment of metal sheet materials
Oleksii Kaglyak 0000-0002-5602-543X, M.V. Romanenko, S.M. Tkachenko, V.V. Romanenko, O.S. Kozyrev, S.S. Saliy
0000-0002-4294-3889, M.I. Anyakin
0000-0002-6615-8471
- National Technical University of Ukraine “Igor Sikorsky Kyiv Polytechnic Institute”
Oral in Person
Laser as an instrument for material treatment is well controllable clear positioned and flexible. This advantages allow to form in sheet materials stresses with determine value and sign on a clear determined location. If residual stresses after heating-cooling cycle exceed the yield point, it`s compensate by plastic deformation. In this case could be provided laser forming process. Controlled energy input and definite irradiation area allows forming sheets in needed shape. From the other hand if residual stresses balanced and don’t reached up yield point, in sheet is being created area with changed properties especially when structure-phase transformation is inherent for treated material. These areas with changed properties could be considered as “metallurgical ribs” and it`s cause increase of rigidity of sheet samples. These “metallurgical ribs” could be oriented towards working load of construction and increase general stability and rigidity of it.
In both cases of laser forming and laser strengthening irradiation was carried out by specific trajectories. During laser forming the trajectories could coincide to increase bending angle, be parallel to form cylindrical shape, placed by certain low to form certain shape. Distance between adjacent laser passes is a process parameter which determine radius of samples curvature as well as number of passes determine bending angle on local trajectory. In case of laser strengthening of sheets irradiated area should be symmetric on both sides of sheet in order to balance residual stresses which shouldn’t exceed the yield point. Another possibility to implement this process is to form even residual stresses distribution over sickness of sheet during one side irradiation. It could be achieved by using special shape of energy distribution across the laser beam as example horseshoe form.
In both processes the result is determined by level and distribution of residual stresses in treated material. The most affective parameters of both processes are power of laser beam, size of focal spot, movement speed of laser beam on sample surface, topography of laser passes, geometry and property of treat materials.
Different materials could be formed by Laser forming: stainless and carbon steels (after rolling and previously hardened), titanium and aluminum alloys. The thickness of sheets which could be formed lies in wide field from foil to more than 6mm. Deviation of forming results during multi-pass laser forming lay under 5%.
During strengthening samples from steels AISI 1010 and AISI 304 an increase in tensile yield strength of 28% was observed. As samples were used sheets with thickness 0.5mm, 0.8mm and 1mm. Which were irradiated from both sides by YAG laser (power range – 350-500 Wt, beam diameter – 4mm, beam moving speed – 4-6.5m/min). After irradiation treated area was cut out using electrical discharge machining as well as not irradiated area with same shape and size to compare tensile test results.