Development of a cored wire based on the Ti–46Nb–2Mo–1.6Zr–1.4Al β-titanium alloy for multilayer TIG deposition
Serhiy Schwab1 0000-0002-4627-9786, Serhii Akhonin1
0000-0002-7746-2946, Valeriy Bilous1
0000-0002-0082-8030, Roman Selin1
0000-0002-2990-1131, Leonad Radchenko1
0009-0008-1097-7137, Volodymyr Tunyk2
0009-0004-3777-5202
- 1E. O. Paton Electric Welding Institute of the NAS of Ukraine
- 2Physico-technological Institute of Metals and Alloys of the NAS of Ukraine
Poster
β-Titanium alloys are a promising class of structural materials combining high specific strength, corrosion resistance, processability, and, compared with α- and α+β-titanium alloys, the possibility of achieving a reduced elastic modulus. Particular interest is focused on metastable β-titanium alloys alloyed with β-stabilizing elements such as Nb and Mo. Alloys of the Ti–Nb–Mo–Zr–Al system are promising for additive manufacturing applications, including the fabrication and repair of components by arc deposition.
This study investigates the fabrication of a powder-cored wire and the structural and mechanical characteristics of multilayer deposits produced using a β-titanium alloy with the composition Ti–46Nb–2Mo–1.6Zr–1.4Al. The initial alloy was produced at the SPC “Tytan” of the E.O. Paton Institute of Electric Welding of the NAS of Ukraine using electron-beam melting with an intermediate crucible. Powder was produced from the obtained alloy by the hydride–dehydride (HDH) process and used to form the core of the powder-cored wire.
A powder-cored wire with a diameter of 3.0 mm and a sheath made of commercially pure titanium was fabricated using the obtained powder. The powder filling ratio of the wire was 55–60%. Multilayer TIG deposition was performed using the fabricated wire as filler material under a previously selected set of process parameters. The deposition speed was 8 m/h, while the wire feeding speed was 30–35 m/h.
X-ray radiographic examination of the deposited sample revealed the presence of pores in the deposited metal. To improve process stability and reduce porosity, a new version of the powder-cored wire was fabricated, in which, in addition to the Ti–46Nb–2Mo–1.6Zr–1.4Al powder, a flux component based on a system of alkali-metal fluorides was introduced into the core. After multilayer TIG deposition using the modified wire, the amount of porosity in the deposited metal was substantially reduced, indicating a positive effect of the flux component on the formation of a dense deposited structure.
The microstructure of the obtained samples was investigated using optical and electron microscopy. The distribution of chemical elements across the cross-section of the deposited metal was determined by EDX analysis using an attachment to a scanning electron microscope. A comparative analysis of the microstructure and microhardness of the samples produced using powder-cored and powder-flux-cored wires was performed.
The obtained results demonstrate the potential of using powder-cored wires based on the β-titanium alloy Ti–46Nb–2Mo–1.6Zr–1.4Al for multilayer TIG deposition. The introduction of a flux component based on alkali-metal fluorides significantly reduces the porosity of the deposited metal and can be used for further optimization of the technology for producing dense multilayer components from β-titanium alloys.