Influence of Weld Geometry Characteristics on the Mechanical Performance of Fiber Laser Welded Dissimilar SS316 Stainless Steel–Inconel 718 Joints
Pravin G. Bhakte1 0009-0009-9760-1729 , D. Narsimhachari1
0000-0002-5833-7590, Inayat Ullah1
0000-0001-5358-1564, M. K. Sharma2
- 1G. H. Raisoni University, Saikheda Madhya Pradesh, India
- 2Bajaj Steel Industries Limited, Nagpur
Oral Online
The dissimilar joining of SS316 stainless steel and Inconel 718 has gained considerable attention in aerospace, nuclear, petrochemical, and power generation industries, where components require a combination of excellent corrosion resistance and high-temperature mechanical performance. However, joining these dissimilar alloys is challenging because of the significant differences in their thermophysical and metallurgical properties, which lead to variations in weld geometry, non-uniform solidification, elemental segregation, residual stress development, and an increased susceptibility to hot cracking, thereby making the fabrication of structurally reliable joints difficult. To address these challenges, the present study, investigated the influence of laser power (2–3 kW) and welding speed (1–5 m/min) on the weld geometry, microstructure, and mechanical behaviour of 2 mm thick SS316–Inconel 718 butt joints fabricated using ER316L filler wire..
The selected welding parameters produced sound joints with complete penetration, favourable weld geometry, a narrow heat-affected zone, and good metallurgical bonding. Variations in laser power and welding speed significantly influenced the weld bead geometry, which subsequently affected the solidification behaviour, microstructural evolution, and mechanical performance of the dissimilar joints. The welded joints exhibited an ultimate tensile strength of approximately 655 MPa , while the fusion zone exhibited an average microhardness of about 220 HV, intermediate between the SS316 base metal (185 HV) and Inconel 718 (406 HV). Microstructural characterization revealed a refined γ-austenitic dendritic matrix containing Nb-rich Laves phase (~19.7 at.% Nb), NbC carbides, and finely dispersed Al₂O₃ inclusions. Nb segregation during solidification promoted the formation of the interdendritic Laves phase, which contributed to local hardness variation and increased the susceptibility to crack initiation, thereby influencing the overall mechanical performance of the welded joints. Fractographic examination revealed predominantly ductile fracture characterized by uniformly distributed dimples with localized cleavage facets. Overall, the study demonstrates that weld geometry characteristics play a significant role in governing the microstructural evolution and mechanical performance of fiber laser welded dissimilar SS316–Inconel 718 joints.
Keywords: Fiber laser welding, Dissimilar welding, SS316 stainless steel, Inconel 718, Structural integrity, .