Fused Deposition Modeling is a widely recognized additive manufacturing technology for producing plastic parts. However, its ability to produce custom plastic or composite details creates new opportunities beyond conventional 3D printing. By creating parts with complex geometries, controlled morphology and patterns, this technology can be adapted for plastic welding and joining.

In current work, the composite filament was produced for FDM 3D printing with further pyroresistive heating of printed samples and welding tests. The filament was based on polylactic acid (PLA) filled with 5 wt.% of carbon nanotubes (CNT) and non-conductive additives. The heating elements had a rectangular shape with dimensions of 10x30x0.3mm (2 layers of thickness, 0.15mm each) without walls and with infill only. The main difference between the series of samples was the pattern of the infill, where both numbers of the labels indicate the angle between the main axis of the sample and the direction of printing. For example, 0-90 means that the first layer was printed along the main axis (30mm) and the second layer was perpendicular. Generally, 5 patterns were printed and tested, namely 0-0, 0-90, 45-45, 45-135, 90-90. Pyroresistive heating was conducted on DC voltages in the range of 0.2 up to 29 Vdc, welded joints were obtained on the custom setup for butt welding.

The study has shown a strong correlation between the pattern of the 3D printed part and its pyroresistive properties. An increase in current on the VA curve denotes the influence of the tunneling effect and the appearance of the negative temperature coefficient. Experimental data provide voltages applied to the samples needed to reach the minimum temperature for welding (200 oC), the values are in the range of 25-29 Vdc. The possibility of welding 3D printed PLA parts with a printed heating element was successfully tested.