Thermodeformation Profile of As-Deposited Nickel-Based Alloys as a New Integral Technological Characteristic for Arc Additive Manufacturing
Mykola Cherviakov 0000-0003-4440-7665, Oleksandr Yarovytsyn
0000-0001-9922-3877, Hanna Zviahintseva
0000-0002-6450-4887, Ivan Volosatov
0000-0003-2593-9869, Heorhii Khrushchov
0000-0002-4045-3587, Dmitro Strezhniev
0009-0005-4721-5361
- Paton Welding Institute of NAS of Ukraine, Kyiv, Ukraine
Oral in Person
Reliable qualification of additive materials for welding arc additive manufacturing requires experimental methods capable of reproducing the thermal and mechanical conditions experienced by multilayer deposited metal. Conventional hot-cracking tests developed for welded joints do not adequately simulate the repeated thermal cycles and relatively low restraint conditions characteristic of additive manufacturing and therefore cannot provide reliable information on the deformation capacity of deposited metal or its susceptibility to hot cracking.
Тhe thermodeformation profile, defined as the temperature dependence of the critical rupture strain of deposited metal in the as-deposited condition, is proposed as a new integral technological characteristic of nickel-based filler materials for arc additive manufacturing. Unlike conventional hot-cracking indices, this thermodeformation characteristic directly characterizes the deformation capacity of multilayer deposited metal under representative arc additive manufacturing conditions and provides a physically meaningful basis for comparative material qualification.
The methodology is based on manufacturing multilayer "vertical wall" deposits by micro-plasma powder welding deposition and TIG deposition, followed by longitudinal high-temperature tensile testing of miniature specimens within the temperature range of 20–1100°C. The obtained thermodeformation profile enables identification of temperature intervals with the highest probability of ductility-dip cracking initiation during repeated thermal cycles and can be applied for comparative assessment of filler materials supplied in powder or wire form.
Eight commercially important nickel-based alloys representing different alloying concepts and strengthening mechanisms – Inconel 625, Hastelloy C22, Inconel 718, EP367, EP648, ChS40, EI698 and René80 – were investigated. The results revealed distinct thermodeformation profiles for different alloy groups. Heat-resistant superalloys with chromium and molybdenum exhibited reduced deformation capacity mainly within the 600–800°C temperature interval, whereas precipitation-hardened nickel superalloys showed progressive widening of the low-ductility range with increasing γ′-phase content. The previously established low ductility of René80 deposited metal in the «as-deposited» condition (ε = 0.8–4.8% within 20–1100°C), together with its high susceptibility to hot cracking, indicates that ductility-dip cracking may develop under restraint conditions when the critical longitudinal rupture strain decreases below 5–10% at 600–1100°C. In contrast, Inconel 718 and EP648 retained comparatively stable thermodeformation behavior, confirming their suitability for arc additive manufacturing.
Elevated oxygen and nitrogen contents inherited from filler materials for arc additive manufacturing significantly reduced the critical rupture strain near the solidus temperature, increasing the probability of ductility-dip, segregation and liquation cracking. Based on the obtained results, recommended impurity limits for nickel-based filler materials are established.
The proposed thermodeformation profile represents a new integral technological characteristic of nickel-based filler materials and suitable deposited metal. It provides a resource-efficient basis for material qualification, comparative assessment and optimization of welding arc additive manufacturing processes employing either powder or wire feedstock.