← Strength and Stress-Strain States of Welded Joints and Structures

Effect of stainless-steel filler metals on the stress corrosion cracking behavior of dissimilar weld joints of 2205/316L.

Teresita del niño Jesús Sánchez Cruz , Antonio Contreras Cuevas (2), Victor Hugo López-Morelos (3), Heriberto Granados Becerra (3), Jorge Antonio G. Sánchez (1), Luis Dzib (1), Orest Bilyy (1)

  1. (1) Instituto de Investigación en Corrosión y Preservación de Materiales, (2) Instituto Mexicano del Petróleo, (3) Instituto de Investigación en Metalurgia y Materiales

Oral Online

The use of dissimilar welded joints offers significant industrial advantages, but selecting the proper welding process and filler metal remains challenging to obtain appropriate mechanical and corrosion performance. In this study, slow strain rate tests were performed on tensile specimens of dissimilar joints of 2205 and 316L stainless steels welded with the pulsed-current gas metal arc process, where two different filler metals were evaluated: ER-309L and ER-316L-Si in a 20 vol.% MgCl₂ solution at 25 °C and 80 °C to assess susceptibility to stress corrosion cracking (SCC). Yield stress and ultimate tensile strength were similar, while the elongation decreased with ER-316L-Si. This finding indicates that the welded joint with ER-309L reduced the susceptibility to stress corrosion cracking. Electrochemical impedance spectroscopy showed that increasing applied stress reduced the impedance modulus and phase angles, indicating greater electrochemical activity at the surface. Overall, the results demonstrate that pulsed-current GMAW with ER-309L filler provides a reliable option for welding 2205/316L dissimilar stainless steels.