FINE STRUCTURE FEATURES OF THE LOW-COST Ti-1.5Fe-0.4O TITANIUM ALLOY

Berdnikova O. 0000-0001-9754-9478, Hryhorenko S. 0000-0003-0625-7010, Titkov Ye. 0000-0003-2735-6923, Kushnarova O. 0000-0002-2125-1795

  1. E.O. Paton Electric Welding Institute of the NAS of Ukraine, Kyiv

Oral in Person

FINE STRUCTURE FEATURES OF THE LOW-COST Ti-1.5Fe-0.4O TITANIUM ALLOY

Hryhorenko S., Titkov Ye., Kushnarova O., Berdnikova O.

E.O. Paton Electric Welding Institute of the NAS of Ukraine, Kyiv, e-mail: [email protected]

This work presents a study of an experimental titanium alloy of the Ti-1.5Fe-0.4O alloying system. The alloy ingots were produced via electron beam melting (EBM) at the Department of Metallurgy and Welding of Titanium Alloys of the E.O. Paton Electric Welding Institute of the National Academy of Sciences of Ukraine. Microstructural features of the experimental alloy samples were investigated at the Department of Physico-Chemical Research of Materials using a JAMP 9500F electron microscope (JEOL, Japan); microhardness was measured using an M-400 tester (LECO, USA) under a load of 0.1 kg. Phase analysis was performed by X-ray diffraction (XRD) using a DRON UM-1 diffractometer. The fine structure at the dislocation level was investigated by transmission electron microscopy (TEM) using a JEM-200CX microscope (JEOL, Japan) at an accelerating voltage of 200 kV.

The Ti-1.5Fe-0.4O alloy (Kβ = 0.34) is a near-α alloy containing a small amount of the β-phase. It was established that the fraction of the α-phase (α-Ti) with lattice parameters a = 2.9501 Å,

c = 4.6785 Å is 90.42%, and that of the β-phase (β-Ti) is 9.58% (a = 3.2137 Å). Inside the polyhedral α-phase grains, a colony (packet) structure with a size of 50–150 μm is observed at a microhardness of HV = 2600 – 2850 MPa. The thickness of the α-phase plates ranges from

3 to 7 μm.

The substructure of the phase constituents and its parameters, the dislocation structure, and the stoichiometric composition of phase particles within the internal volumes of the alloy structure were investigated by TEM. Constituents in the form of lath (plate-like) α′ and β phases are observed, with thicknesses of 0.4–2.14 μm for α′ plates and 0.06–0.35 μm for β plates. Within the plate-like structures, a substructure with dimensions of 0.12–0.47 × 0.3–1.35 μm is formed. The dislocation density exhibits a uniform distribution (ranging from 3×109–7×109 cm-2 to 2×1010–3×1010 cm-2). Intermetallic and oxide particles are formed within the alloy structure: Fe2Ti (10–40 nm in size); Ti3O5 (10–30 × 100 nm); FeTiO5 (70–90 nm); and Ti4Fe2O (10–60 nm). The formation of phase nanoparticles within the fine-plate structure and substructure, combined with a uniform dislocation density distribution, provides the required level of strength and ductility in the experimental Ti-1.5Fe-0.4O titanium alloy.