Phase equilibria in the Al-Ni-Ti system as a scientific basis for the development of high-performance alloys
Kostyantyn Korniyenko 0000-0002-4459-6681
- Frantsevich Institute for Problems of Materials Science, NAS of Ukraine, Kyiv
Poster
The Al-Ni-Ti alloys have emerged as a promising class of materials due to their exceptional combination of high-temperature strength, oxidation resistance and creep resistance. These properties make them ideal candidates for various applications in aerospace engineering, biomedical engineering and other demanding fields. The search for new materials containing these metals opens up opportunities for establishing of optimal combinations and complementarities of positive properties inherent in them. For this purpose information about phase equilibria in the corresponding systems is necessary.
Data on phase relations in the Al-Ni-Ti system are presented in the literature in quite detail. Formation of the six ternary compounds was established. Liquidus surface, Scheil diagram, isothermal sections in the temperature range 1350 to 600°C and series of vertical sections were constructed. 21 four-phase invariant equilibria with participation of liquid phase take place in the system.
The alloying potential of nickel as a minor constituent has been investigated in TiAl-based intermetallics with respect to its constitutional ability to provide the necessary microstructures for higher ductility and low fracture toughness. As a result of compression tests of the Ti25Ni8Al67 (at.%) alloy, it has a yield strength of 355 MPa at room temperature and can exhibit substantial plasticity. A way to obtain high-strength in high temperature structural Ni50-xTi50Alx (x = 6, 7, 8, 9; in at.%) alloys with controlled Al addition to change the volume fraction, the shape, and the distribution of strengthening phases was proposed. A yield stress of 1800 MPa and more than 10% of compression strain were achieved at room temperature; and a yield stress of 400 MPa at 800°C. The Ni71Ti7Al22 (at.%) eutectic alloy with a dual-phase lamellar microstructure possesses an ultra-high fracture strength of 3500 MPa and an admirable fracture strain of 30% under compression at room temperature. It also possesses a super-high strength of 1180 MPa at 700°C. The superior mechanical property can be attributed to the synergetic deformation of the eutectic structure, R characterization (abnormal yield effect) and the Ti alloying enhanced phase stability at elevated temperatures. The non-equilibrium solidification induced supersaturation also results in the super-high strength at room-to-medium temperature and a unique softening mechanism via the formation of the two-fold composite structure. These results provide a promising candidate alloy for elevated-temperature applications, and a new paradigm for dual-intermetallic eutectic alloy design.